[1]刘啟迪,周真明,张红忠,等.煅烧改性净水厂污泥制备除磷材料工艺参数优化[J].华侨大学学报(自然科学版),2018,39(1):51-56.[doi:10.11830/ISSN.1000-5013.201704049]
 LIU Qidi,ZHOU Zhenming,ZHANG Hongzhong,et al.Parameter Optimization of Preparing Phosphorus Removal Material by Using Calcined Water Treatment Plant Sludge[J].Journal of Huaqiao University(Natural Science),2018,39(1):51-56.[doi:10.11830/ISSN.1000-5013.201704049]
点击复制

煅烧改性净水厂污泥制备除磷材料工艺参数优化()
分享到:

《华侨大学学报(自然科学版)》[ISSN:1000-5013/CN:35-1079/N]

卷:
第39卷
期数:
2018年第1期
页码:
51-56
栏目:
出版日期:
2018-01-17

文章信息/Info

Title:
Parameter Optimization of Preparing Phosphorus Removal Material by Using Calcined Water Treatment Plant Sludge
文章编号:
1000-5013(2018)01-0051-06
作者:
刘啟迪1 周真明1 张红忠2费霞丽3 谢保金4 李书文1 苑宝玲1
1. 华侨大学 土木工程学院, 福建 厦门 361021;2. 泉州市自来水有限公司, 福建 泉州 362000;3. 厦门水务集团有限公司, 福建 厦门 361008;4. 厦门水务中环制水有限公司 制水三部, 福建 厦门 361000
Author(s):
LIU Qidi1 ZHOU Zhenming1 ZHANG Hongzhong2 FEI Xiali3 XIE Baojin4 LI Shuwen1 YUAN Baoling1
1. College of Civil Engineering, Huaqiao University, Xiamen 361021, China; 2. Quanzhou Water Limited Company, Quanzhou 362000, China; 3. Xiamen Water Group Limited Company, Xiamen 361008, China; 4. The Third Sector, Water Production Subsidiary Company of Xiamen Water Group Limited Company, Xiamen 361000, China
关键词:
净水厂污泥 煅烧改性 工艺参数 除磷材料
Keywords:
water treatment plant sludge calcined modification technological parameter phosphorus removal material
分类号:
X524
DOI:
10.11830/ISSN.1000-5013.201704049
文献标志码:
A
摘要:
针对净水厂污泥(WTPS)直接应用于富营养化水体除磷过程中存在向水体释放氨氮和有机物的问题,研究煅烧改性净水厂污泥(C-WTPS)制备除磷材料的可行性,考察C-WTPS的氨氮和有机物的释放情况,优化煅烧工艺参数.等温吸附试验和去离子水浸渍试验的结果表明:在煅烧温度为50~400 ℃,煅烧时间为0.5~4.0 h范围内,最佳煅烧温度为400 ℃,最佳煅烧时间为2.5 h;与WTPS相比,C-WTPS对磷的吸附量增长48.2%,氨氮和总有机碳(TOC)的释放量分别削减79.5%,71.9%,铵态氮和有机物的质量比分别削减80.5%,91.6%;C-WTPS制备除磷材料具有可行性,煅烧改性工艺不仅提高WTPS的磷吸附能力,而且大为削减了WTPS氨氮和有机物的释放量.
Abstract:
Since ammonia nitrogen and organic matter release in the process of phosphorus removal in eutrophic water by using water treatment plant sludge(WTPS), the feasibility of preparing phosphorus removal material by using calcined water treatment plant sludge(C-WTPS)was studied. In addition, the release of ammonium nitrogen and organic matter of C-WTPS was investigated, and the technological parameters were opt- imized. The results of isothermal adsorption experiments and deionized water dipping tests showed that the optimum calcination parameters were calcining temperature at 400 ℃ and calcining time with 2.5 h in the range of calcining temperature between 50 to 400 ℃ and calcining time from 0.5 to 4.0 h. Comparing with WTPS, the phosphorus adsorption capacity of C-WTPS improved 48.2%, the release capacities of ammonia nitrogen and total organic carbon(TOC)of C-WTPS were reduced 79.5% and 71.9% respectively, and the contents of ammonium nitrogen and organic matter of C-WTPS were reduced 80.5% and 91.6% respectively. Therefore, it is feasible to prepare phosphorus removal material by using C-WTPS. Calcining process not only improves the phosphorus adsorption capacity of WTPS, but also reduces the release capacities of ammonia nitrogen and organic matter significantly.

参考文献/References:

[1] SMITH V H,SCHINDLER D W.Eutrophication science: Where do we go from here?[J].Trends in Ecology and Evolution,2009,24(4):201-207.DOI:10.1016/j.tree.2008.11.009.
[2] SCHINDLER D W,CARPENTER S R,CHAPRA S C,et al.Reducing phosphorus to curb lake eutrophication is a success[J].Environmental Science and Technology,2016,50(17):8923-8929.DOI:10.1021/acs.est.6b02204.
[3] HUSER B J,EGEMOSE S,HARPER H,et al.Longevity and effectiveness of aluminum addition to reduce sediment phosphorus release and restore lake water quality[J].Water Research,2016,97:122-132.
[4] IMMERS A K,BAKKER E S,DONK E V,et al.Fighting internal phosphorus loading: An evaluation of the large scale application of gradual Fe-addition to a shallow peat lake[J].Ecological Engineering,2015,83:78-89.DOI:10.1016/j.ecoleng.2015.05.034.
[5] GERLINDE W,THOMAS G,MICHAEL H,et al.Phosphorus balance of Lake Tiefwarensee during and after restoration by hypolimnetic treatment with aluminum and calcium salts[J].Lake and Reservoir Management,2009,25(4):377-388.DOI:10.1080/07438140903238591.
[6] DOUGLAS G B,LURLING M,SPEARS B M.Assessment of changes in potential nutrient limitation in an impounded river after application of lanthanum-modified bentonite[J].Water Research,2016,97:47-54.DOI:10.1016/j.watres.2016.02.005.
[7] 穆凯艳,赵田甜,张樱美,等.膨润土载锆除磷复合材料的研究[J].环境工程,2014,32(3):60-64.DOI:10.13205/j.hjgc.201403015.
[8] 王卫东,郝瑞霞,张晓娴,等.高效磷吸附剂Mg/Al-LDO的制备及除磷机制[J].环境科学,2017,38(2):572-579.DOI:10.13227/j.hjkx.201606187.
[9] 刘焱,吴玲琳,王世和,等.工业废渣基除磷材料的静态吸附研究[J].环境工程学报,2009,3(2):275-278.
[10] 帖靖玺,赵莉,张仙娥.净水厂污泥的磷吸附特性研究[J].环境科学与技术,2009,32(6):149-151.DOI:10.3969/j.issn.1003-6504.2009.06.034.
[11] 王昌辉,裴元生.给水处理厂废弃铁铝泥对正磷酸盐的吸附特征[J].环境科学,2011,32(8):2371-2377.
[12] 黄华山,杨志敏,周真明,等.净水厂污泥覆盖控制底泥氮磷释放效果[J].华侨大学学报(自然科学版),2016,37(3):347-351.DOI:10.11830/ISSN.1000-5013.2016.03.0347.
[13] 国家环境保护总局.水和废水监测分析方法[M].4版.北京:中国环境科学出版社,2002.
[14] 金相灿,屠清瑛.湖泊富营养化调查规范[M].2版.北京:中国环境科学出版社,1990.
[15] 鲍士旦.土壤农化分析[M].3版.北京:中国农业出版社,2005.
[16] GONZáLEZ M J J,PéREZ C B,FERNáNDEZ G E.Analytical phosphorus fractionation in sewage sludge and sediment samples[J].Analytical and Bioanalytical Chemistry,2005,381(4):873-878.DOI:10.1007/s00216-004-2989-z.
[17] 吴慧芳,胡文华.聚合氯化铝污泥吸附除磷的改性研究[J].中国环境科学,2011,31(8):1289-1294.
[18] 高思佳,王昌辉,裴元生.热活化和酸活化给水处理厂废弃铁铝泥的吸磷效果[J].环境科学学报,2012,32(3):606-611.
[19] YANG Y,ZHAO Yaqian,BABATUNDE A O,et al.Characteristics and mechanisms of phosphate adsorption on dewatered alum sludge[J].Separation and Purification Technology,2006,51(2):193-200.DOI:10.1016/j.seppur.2006.01.013.
[20] ICHIHARA M,NISHIO T.Suppression of phosphorus release from sediments using water clarifier sludge as capping material[J].Environmental Technology,2013,34(15):2291-2299.DOI:10.1080/09593330.2013.765924.

备注/Memo

备注/Memo:
收稿日期: 2017-04-26
通信作者: 周真明(1981-),男,副教授,博士,主要从事水体富营养化控制理论与技术的研究.E-mail:zhenming@hqu.edu.cn.
基金项目: 国家科技支撑计划项目(2015BAL01B01); 福建省泉州市科技计划重点项目(2014Z128); 华侨大学中青年教师科研提升资助计划项目(ZQN-PY313)http://www.hdxb.hqu.edu.cn
更新日期/Last Update: 2018-01-20